Corrosion will generally NOT occur on a steel substrate when Inert gases may be placed in confined spaces to reduce or prevent corrosion. New steel is not hom*ogenous and contains Carbon steel will generally corrode if it is electrically connected in the presence of a suitable electrolyte with Which of the following is anodic with respect to carbon steel when in a seawater electrolyte? Chemical salts dissolved in an electrolyte generally contribute to corrosion by The rate of corrosion occurring at a hole, scratch, or other discontinuity of a coating film may be affected by I. the presence of an electrolyte II. adherent mill scale on the substrate III. the anode is in contact with the atmosphere The use of an incorrect thinner may cause a coating to Coatings can control corrosion of steel by I. preventing electrolytes from contacting the metal surface. II. sacrificing themselves to protect the steel substrate. III. supplying inhibitors to passivate the metal surface. The vehicle of a coating consists of I. solvent, binder, and liquid additives. II. solvent only. III. binder and pigment. Inspection reports should address the A typical daily report will include I. description of equipment and manpower. II. explanation of work stoppages. III. ambient conditions. IV. inspector’s opinion of the contractor. The required sequence of work within a specification on a project is Solvents are added to coating formulations to Most organic coatings are Inspection reports should include which of the following? I. Environmental conditions II. Details of surface cleaning and materials III. Coatings application Which items are the basic principles in documentation by the inspector? I. Reports are written in ink II. No blank spaces III. Reports should be signed IV. Reports must be printed Inspector’s daily reports are used for which of the following? I. By the contractor to estimate the amount of work done that day II. To provide continuity between inspectors. III. To aid in arbitration between the contractor and client IV. To help in cases of a coating failure A pre-job conference is helpful for reviewing I. safety procedures. II. cleaning operations. III. application procedures. The inspector’s method of marking defects In case of conflict or a difference of opinion, the coating inspector needs to All bidders on a coating job should I. attend the pre-bid meeting. II. be given a copy of the pre-job minutes. III. attend the pre-job conference. IV. be allowed a walk-through of the project. Before attending a pre-job conference, the coating inspector should I. read and understand the specification. II. identify problems with the specification. III. walk through the work site. The coating contractor’s questions about enforcing the coating specification should best be brought up The coating inspector should act as a recording secretary during the pre-job meeting. A sling psychrometer directly measures Steel surface temperature during coating application should be Dew point is measured and calculated by using The Dew point is the temperature at which A decrease in temperature will generally cause the corrosion rate to I. increase. II. decrease. III. remain constant. The presence of certain salt deposits such as ferrous sulfate or ferrous hydroxides may be determined by which of the following? Workers exposed to hazardous levels of free silica dust such as released during the sandblast cleaning process may develop silicosis, which is a disease of the ISO 8503-1 comparator are available for which of the following abrasives? I. Sand II. Grit III. Shot Which of the following statements concerning ultra-high pressure water jetting is true? I. Production rates are cost-effective. II. Seldom used for surface preparation. III. Often used for surface preparation. IV. Lower pressure will not remove the tight mill scale. Coating operations should NOT take place unless the substrate surface temperature is At least The cathode of a corrosion cell Nozzle pressure for manual blast cleaning is generally accepted to be Extra-coarse Testex replica tape is used when it is expected that the depth of the anchor pattern/surface profile to be measured will be 3 mils (75 microns). When following a specification for surface preparation standards, the inspector should NOT? If the coating inspector finds that the coating was applied thicker than specified, he/she should 33 feet is approximately how many meters? The requirements of a project should be defined by the The coating inspector should require white metal surface preparation if A well-written coating specification should contain information regarding I. surface preparation standards. II. safety. III. locations to be coated. If the desired DFT of a coating is 100 microns (4 mils), what wet film thickness will be required if the coating contains 100% volume solids? It is the coating inspector’s responsibility to The coating inspector’s responsibility is to It is the coating inspector’s responsibility to The coating inspector’s responsibility is to Inspection of mixing and thinning operations is important An inspector’s primary duty is to I. observe the actions of the contractor. II. report actions of the contractor. III. document actions of the contractor. IV. enforce all safety rules. Corrosion is slower in hot environments than in cool ones. Accidental injection through the skin by airless spray If the inspector observes coatings or solvents being applied to a surface, through an air hose, in an Air Spray system he/she should I. look for other signs of poor practice. II. notify the foreman. III. record findings in a log book. With conventional air spray equipment, the dry spray may be caused by “Arcing” a spray gun may cause I. uneven application. II. a spark hazard. III. excessive overspray. Which of the following is an advantage of airless spray compared to conventional air spray? Always ground the fluid hose used in an airless spray to The use of respiratory equipment is not necessary when spray painting. Many liquid coatings The presence of oil or moisture in compressed air Conventional air spray guns have adjustments for According to NACE RP0188-99, the search electrode of a high-voltage holiday detector should be moved across the surface at approximately According to SSPC-PA 2, always calibrate magnetic DFT (Type 1) gauges The paint inspection gauge (“Tooke” gauge) is a destructive test instrument. Generally, applicators do NOT need respirators when spray painting. Fluid pressure in a conventional air spray fluid line is controlled by Check for holidays using a Nondestructive test instruments, properly used High-voltage DC holiday detectors are used to test All magnetic DFT instrument magnets or probes must be held at a right angle to the painted surface to produce valid measurements. Which of the following are the principal advantages of abrasive-injected water blast over water washing? I. Increased profile II. Increased production III. Reduced manpower There is no spark hazard associated with holiday test equipment. Always ground low-voltage DC holiday detectors to Magnetic DFT instruments Air temperature has no effect up on relative humidity. Where will you find information such as ingredients, exposure limits, and flammability classifications of coatings? Which items of information are generally found on product data sheets? I. Solids by volume II. VOC values III. Chemical composition Which items found on a product data-sheet provide application information? I. Cure time II. Profile III. Tip size IV. Recoat interval When applying coatings, instructions regarding appropriate types of Personal Protective Equipment (PPE) will be found within the The Material Safety Data Sheets (MSDS) I. are not required to be maintained at the job site. II. lists the health hazards of the material. III. lists the protective equipment required during application. Which of the following is a type of coating defect that occurs when each brush stroke or spray gun pass is visible after the coating has cured? Osmotic blistering is most likely to occur as a result of Intercoat delamination may be reduced by If a coating that cures by chemically-induced polymerization is applied without the converter having been added first the Chalking The type of coating that cures by heat-induced polymerization is Which of the following coating types are often supplied in two components? Phenolic coatings are very flexible. Curling or lifting can be caused by I. solvent attacking an existing coating film. II. application of an incompatible coating over an existing coating. III. deterioration of a paint film due to old age. Chalking is best described as Failure to add the converter to the base before application of a coating that cures by chemically induced polymerization may result in To extend the pot-life of an epoxy coating the applicator may The percentage of metallic zinc dust by weight in the dried film of a zinc-rich coating is generally Coatings that cure by oxidation are Amine blush is an amber oily film, which occurs on Oil-based coatings A pigment is The most important property of a primer for steel is its ability to “Kick-out” occurs when An epoxy ester coating is a one-package coating that cures by

Here You can Take A Free NACE CIP Level 1 Exam Practice Test, with Latest NACE (CIP) Coating Inspector Program Level 1 Question and Answers

1.

Corrosion will generally NOT occur on a steel substrate when

2.

Inert gases may be placed in confined spaces to reduce or prevent corrosion.

3.

New steel is not hom*ogenous and contains

4.

Carbon steel will generally corrode if it is electrically connected in the presence of a suitable electrolyte with

5.

Which of the following is anodic with respect to carbon steel when in a seawater electrolyte?

6.

Chemical salts dissolved in an electrolyte generally contribute to corrosion by

7.

The rate of corrosion occurring at a hole, scratch, or other discontinuity of a coating film may be affected by
I. the presence of an electrolyte
II. adherent mill scale on the substrate
III. the anode is in contact with the atmosphere

8.

The use of an incorrect thinner may cause a coating to

9.

Coatings can control corrosion of steel by
I. preventing electrolytes from contacting the metal surface.
II. sacrificing themselves to protect the steel substrate.
III. supplying inhibitors to passivate the metal surface.

10.

The vehicle of a coating consists of
I. solvent, binder, and liquid additives.
II. solvent only.
III. binder and pigment.

11.

Inspection reports should address the

12.

A typical daily report will include
I. description of equipment and manpower.
II. explanation of work stoppages.
III. ambient conditions.
IV. inspector’s opinion of the contractor.

13.

The required sequence of work within a specification on a project is

14.

Solvents are added to coating formulations to

15.

Most organic coatings are

16.

Inspection reports should include which of the following?
I. Environmental conditions
II. Details of surface cleaning and materials
III. Coatings application

17.

Which items are the basic principles in documentation by the inspector?
I. Reports are written in ink
II. No blank spaces
III. Reports should be signed
IV. Reports must be printed

18.

Inspector’s daily reports are used for which of the following?
I. By the contractor to estimate the amount of work done that day
II. To provide continuity between inspectors.
III. To aid in arbitration between the contractor and client
IV. To help in cases of a coating failure

19.

A pre-job conference is helpful for reviewing
I. safety procedures.
II. cleaning operations.
III. application procedures.

20.

The inspector’s method of marking defects

21.

In case of conflict or a difference of opinion, the coating inspector needs to

22.

All bidders on a coating job should
I. attend the pre-bid meeting.
II. be given a copy of the pre-job minutes.
III. attend the pre-job conference.
IV. be allowed a walk-through of the project.

23.

Before attending a pre-job conference, the coating inspector should
I. read and understand the specification.
II. identify problems with the specification.
III. walk through the work site.

24.

The coating contractor’s questions about enforcing the coating specification should best be brought up

25.

The coating inspector should act as a recording secretary during the pre-job meeting.

26.

A sling psychrometer directly measures

27.

Steel surface temperature during coating application should be

28.

Dew point is measured and calculated by using

29.

The Dew point is the temperature at which

30.

A decrease in temperature will generally cause the corrosion rate to
I. increase.
II. decrease.
III. remain constant.

31.

The presence of certain salt deposits such as ferrous sulfate or ferrous hydroxides may be determined by which of the following?

32.

Workers exposed to hazardous levels of free silica dust such as released during the sandblast cleaning process may develop silicosis, which is a disease of the

33.

ISO 8503-1 comparator are available for which of the following abrasives?
I. Sand
II. Grit
III. Shot

34.

Which of the following statements concerning ultra-high pressure water jetting is true?
I. Production rates are cost-effective.
II. Seldom used for surface preparation.
III. Often used for surface preparation.
IV. Lower pressure will not remove the tight mill scale.

35.

Coating operations should NOT take place unless the substrate surface temperature is At least

36.

The cathode of a corrosion cell

37.

Nozzle pressure for manual blast cleaning is generally accepted to be

38.

Extra-coarse Testex replica tape is used when it is expected that the depth of the anchor pattern/surface profile to be measured will be 3 mils (75 microns).

39.

When following a specification for surface preparation standards, the inspector should NOT?

40.

If the coating inspector finds that the coating was applied thicker than specified, he/she should

41.

33 feet is approximately how many meters?

42.

The requirements of a project should be defined by the

43.

The coating inspector should require white metal surface preparation if

44.

A well-written coating specification should contain information regarding
I. surface preparation standards.
II. safety.
III. locations to be coated.

45.

If the desired DFT of a coating is 100 microns (4 mils), what wet film thickness will be required if the coating contains 100% volume solids?

46.

It is the coating inspector’s responsibility to

47.

The coating inspector’s responsibility is to

48.

It is the coating inspector’s responsibility to

49.

The coating inspector’s responsibility is to

50.

Inspection of mixing and thinning operations is important

51.

An inspector’s primary duty is to
I. observe the actions of the contractor.
II. report actions of the contractor.
III. document actions of the contractor.
IV. enforce all safety rules.

52.

Corrosion is slower in hot environments than in cool ones.

53.

Accidental injection through the skin by airless spray

54.

If the inspector observes coatings or solvents being applied to a surface, through an air hose, in an Air Spray system he/she should
I. look for other signs of poor practice.
II. notify the foreman.
III. record findings in a log book.

55.

With conventional air spray equipment, the dry spray may be caused by

56.

“Arcing” a spray gun may cause
I. uneven application.
II. a spark hazard.
III. excessive overspray.

57.

Which of the following is an advantage of airless spray compared to conventional air spray?

58.

Always ground the fluid hose used in an airless spray to

59.

The use of respiratory equipment is not necessary when spray painting.

60.

Many liquid coatings

61.

The presence of oil or moisture in compressed air

62.

Conventional air spray guns have adjustments for

63.

According to NACE RP0188-99, the search electrode of a high-voltage holiday detector should be moved across the surface at approximately

64.

According to SSPC-PA 2, always calibrate magnetic DFT (Type 1) gauges

65.

The paint inspection gauge (“Tooke” gauge) is a destructive test instrument.

66.

Generally, applicators do NOT need respirators when spray painting.

67.

Fluid pressure in a conventional air spray fluid line is controlled by

68.

Check for holidays using a

69.

Nondestructive test instruments, properly used

70.

High-voltage DC holiday detectors are used to test

71.

All magnetic DFT instrument magnets or probes must be held at a right angle to the painted surface to produce valid measurements.

72.

Which of the following are the principal advantages of abrasive-injected water blast over water washing?
I. Increased profile
II. Increased production
III. Reduced manpower

73.

There is no spark hazard associated with holiday test equipment.

74.

Always ground low-voltage DC holiday detectors to

75.

Magnetic DFT instruments

76.

Air temperature has no effect up on relative humidity.

77. Depth of anchor pattern/surface profile will not affect DFT readings.

78.

Where will you find information such as ingredients, exposure limits, and flammability classifications of coatings?

79.

Which items of information are generally found on product data sheets?
I. Solids by volume
II. VOC values
III. Chemical composition

80.

Which items found on a product data-sheet provide application information?
I. Cure time
II. Profile
III. Tip size
IV. Recoat interval

81.

When applying coatings, instructions regarding appropriate types of Personal Protective Equipment (PPE) will be found within the

82.

The Material Safety Data Sheets (MSDS)
I. are not required to be maintained at the job site.
II. lists the health hazards of the material.
III. lists the protective equipment required during
application.

83.

Which of the following is a type of coating defect that occurs when each brush stroke or spray gun pass is visible after the coating has cured?

84.

Osmotic blistering is most likely to occur as a result of

85.

Intercoat delamination may be reduced by

86.

If a coating that cures by chemically-induced polymerization is applied without the converter having been added first the

87.

Chalking

88.

The type of coating that cures by heat-induced polymerization is

89.

Which of the following coating types are often supplied in two components?

90.

Phenolic coatings are very flexible.

91.

Curling or lifting can be caused by
I. solvent attacking an existing coating film.
II. application of an incompatible coating over an existing coating.
III. deterioration of a paint film due to old age.

92.

Chalking is best described as

93.

Failure to add the converter to the base before application of a coating that cures by chemically induced polymerization may result in

94.

To extend the pot-life of an epoxy coating the applicator may

95.

The percentage of metallic zinc dust by weight in the dried film of a zinc-rich coating is generally

96.

Coatings that cure by oxidation are

97.

Amine blush is an amber oily film, which occurs on

98.

Oil-based coatings

99.

A pigment is

100.

The most important property of a primer for steel is its ability to

101.

“Kick-out” occurs when

102.

An epoxy ester coating is a one-package coating that cures by

Question 1 of 102

Take A Free NACE CIP Level 1 Exam Practice Test - Quiz Course (2024)
Top Articles
Latest Posts
Article information

Author: Moshe Kshlerin

Last Updated:

Views: 6017

Rating: 4.7 / 5 (77 voted)

Reviews: 92% of readers found this page helpful

Author information

Name: Moshe Kshlerin

Birthday: 1994-01-25

Address: Suite 609 315 Lupita Unions, Ronnieburgh, MI 62697

Phone: +2424755286529

Job: District Education Designer

Hobby: Yoga, Gunsmithing, Singing, 3D printing, Nordic skating, Soapmaking, Juggling

Introduction: My name is Moshe Kshlerin, I am a gleaming, attractive, outstanding, pleasant, delightful, outstanding, famous person who loves writing and wants to share my knowledge and understanding with you.